Abstract

Soils in permafrost regions may undergo significant subsidence due to thawing. Oil well surface casing embedded in such soils may be subjected to strains well beyond yield, whatever the casing properties might be. To deal with this, the State of Alaska has issued a specification defining the amount of axial strain that the casing, together with its connectors, must be able to withstand without parting. This paper presents full-scale tension and compression test data demonstrating that a particular weight and grade of 20-in. casing with premium weld-on connectors is a system exceeding those requirements. It is shown that, in tension, the material ultimate strength is reached first in the casing. Similarly, it is shown that, in compression, the casing buckles plastically before the connector fails.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.