Abstract
Both forsterite (Mg2SiO4) and enstatite (MgSiO3) enter a post‐oxide phase characterized by the orthorhombic perovskite structure when subjected to high pressure and temperature in the diamond‐anvil press coupled with laser heating. The lattice parameters for the perovskite phase of MgSiO3 are ao = 4.790 ± 0.002, bo = 4.943 ± 0.002, and co = 6.897 ± 0.003 Å with Z = 4. The calculated density of MgSiO3 (perovskite) is thus 4.083 g/cm³, or 2.8% denser than its isochemical mixed oxides with rocksalt and rutile structures. The density of a mixture of MgSiO3 (perovskite) plus MgO (periclase) is 1.9% greater than that of the mixed oxides with the forsterite stoichiometry.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.