Abstract
Shape-memory polymers are highly desirable in implant biomaterials for minimally invasive surgical procedures. However, most of them lack suitable transition temperature, mechanical properties, and biodegradability. Here, a series of shape-memory polyurethanes are synthesized by postcrosslinking in hard-segment domains using a flexible crosslinker. The materials used are all nontoxic and biodegradable. Through postcrosslinking of unsaturated linear polyurethanes with flexible and biodegradable crosslinker, the crosslinked polyurethanes (CPUs) show good mechanical properties, excellent shape-memory property, and repeatability. The post-crosslinking structure and shape-memory mechanism of CPUs are investigated by Fourier transform infrared spectroscopy, differential scanning calorimetry, and dynamic mechanical analysis tests. The crosslinker endows the fixed phase enough crosslinking and inserts in the hard segments to give the fixed phase certain elasticity. The elastic hard segments make them form more hydrogen bonds with soft segments during shape deformation. The low-molecular-weight poly (ε-caprolactone) offers the samples a shape-memory transition temperature at around 37 °C, which is suitable for implant devices in vivo. This work expands CPUs with an elastic crosslinking structure as potential candidates for implant biomaterials. Since the post-crosslinking polymerization is facile, it can be convenient for industrial production.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.