Abstract

La 0.67Ca 0.33MnO 3 thin films have been grown on 10°, 15°, and 20° vicinal cut SrTiO 3 (1 0 0) substrates by pulse laser deposition. The single phase and the least textured growth have been studied by X-ray diffraction analysis. The post annealing effect with high temperature and high oxygen pressure on the transport properties of films has been investigated by resistance versus temperature measurements. Films with post annealing show large enhancement of metal–insulator transition temperature T p about 20–30 K towards higher temperature and obvious decrease of resistance, which is attributed to the refilling of oxygen, the change of Mn–O–Mn angle and the improvement of crystallinity by the post annealing effect. Specially, film on 20° vicinal cut substrate exhibits the biggest range gap of peak resistance drop, which may originate from more defects caused by steps at this tilt angle and many of these defects are removed after post annealing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.