Abstract

The type of aqueous solution used to wash the enamel surface immediately after etching with orthophosphoric acid affected the tensile bond strength obtained. Washing with a 1% potassium chloride solution was found to effect an improved bond strength, but no difference was observed when different types of water were employed for this purpose. A similar finding of no difference in bond strength was obtained when the possible influence of electrostatic forces was eliminated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.