Abstract
The aim of the work was to identify the possibility of using under extreme conditions parts made of inexpensive steel, protected by sequentially deposited films — Cr and then simultaneously TiN + CrN, micron thickness. Steel grade St3 (Fe ~ 97%) was chosen as the basis. In our country, as in many others, this steel is not only the most common structural material with easy processing and low cost, but also produced in large volumes. The deposition of two consecutive layers of films — Cr and TiN + CrN on steel substrates was carried out using vacuum-arc technology (Arc-PVD). The measurements were carried out after the process of periodic heating of the samples to a temperature of 650 0C, followed by rapid cooling, implemented by immersing the samples in water. The main parameters of the coating were measured — wear resistance, heat resistance, microhardness. Each thermal effect lasted 20 hours, and the entire heating-cooling process was carried out 5 times. The results obtained in this work can be considered very promising for the protection of inexpensive steels.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Bulletin of the Karaganda University "Physics Series"
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.