Porous TiAl alloys with different nominal powder compositions were fabricated through a cost-effective powder metallurgy (PM) approach by sintering TiH2 and Al mixed powders. It is found that the pore properties vary with the TiH2 and Al contents, i.e., the nature of the pores can be improved by using different compositions. Furthermore, by detailed structural characterizations, four crystalline phases, i.e., α2-Ti3Al, γ-TiAl, TiAl3, and Ti2Al5, were observed in the fabricated porous TiAl alloys with different compositions. An optimal composition of TiH2-50wt% Al is preferred since its maximum open porosity is about 70% and its viscous permeability coefficient for nitrogen is 1.11 μm2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.