Abstract

With nano-alumina modified by the fat acid as an inorganic template for making pores, a new kind of porous resin particle with the large surface was synthesized by emulsion polymerization. Moreover, the sulfonated polystyrene resin was fluorinated to increase its acid strength up to Ho 8.6 and the acid amount of 4.1mmol/g. The ratio of butane to water was increased by packing the catalytic resin with the fixed beds of four stages. Under reaction temperature of 168-174°C, butane to water ratio of 2 mol/mol and WHSV1.0 h-1, hydration reaction conversion was over 15 wt%, with the butyl alcohol selectivity of 99 wt% and a good thermal stability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.