Abstract

AbstractPore wall thinning of mesoporous 4H‐SiC by sacrificial oxidation is performed. The dimensions within the as‐etched porous SiC are reduced during dry oxidation at 1100 °C by consuming SiC and removing the grown SiO2 in the subsequent hydrofluoric acid (HF) dip step. The process reduces the average pore wall thickness from 27 nm to approximately 16 nm and reduces the thickness standard deviation from ±5 to ±1.4 nm for the investigated 9 h oxidation interval. The new pore wall thinning method will enable controlled nanoscale size reduction capability for mesoporous 4H‐SiC derived nanostructures.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.