Abstract
AbstractPolyurethanes containing binaphthyl groups were synthesized by reaction of diisocyanates – 4,4'‐diphenylmethane diisocyanate (MDI), 2,4‐toluylene diisocyanate (TDI) and hexamethylene diisocyanate (HDI) – with 2,2'‐(1,1'‐binaphthyl‐4,4'‐ylenedioxy)diethanol (3). The polyurethane obtained from 3 with MDI has an intrinsic viscosity [η]90DMSO90°C of 0,14 dl · g−1 and a melting point of 244 – 260°C, that from 3 with TDI has an [η]90°CDMSO of 0,12 dl · g−1 and a melting point of 181 – 191°C, and that from 3 with HDI has an [η]90°CDMSO of 0,11 dl · g−1 and a melting point of 222 – 241°C. These polymers were found to be crystalline. Segmented polyurethanes (SPU) from 3 with prepolymers of poly(tetramethylene glycol) (PTG), (M = 1079) and MDI or HDI (mole ratio PTG:MDI (or HDI) = 1:2) were also synthesized. The SPU from MDI has an intrinsic viscosity [η]90°CDMSO of 0,56 dl · g−1 and a melting point of 260–275°C, and that from HDI has an [η]90°CDMSO of 0,50 dl · g−1 and a melting point of 231 – 253°C. These polymers show slight crystallinity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.