Carbon nanotubes (CNTs) were deposited on the surfaces of polyurethane (PUR) foams by electrophoretic deposition (EPD). The parameters of EPD were optimized in order to obtain homogeneous CNT coatings on PUR foams and adequate infiltration of the three-dimensional (3D) porous network. The microstructure of the composites was investigated by high-resolution scanning electron microscopy (HRSEM), revealing that optimal quality of the coatings was achieved by an EPD voltage of 20 V. The thermal properties of the CNT-coated specimens, determined by thermogravimetric analysis (TGA), were correlated to the foam microstructure. In vitro tests in concentrated simulated body fluid (1.5 SBF) were performed to study the influence of the presence of CNTs on the bioactivity of PUR-based scaffolds, assessed by the formation of calcium phosphate (CaP) compounds, e.g. hydroxyapatite (HA), on the foam surfaces. It was observed that CNTs accelerate the precipitation of CaP, which is thought to be due to the presence of more nucleation centres for crystal nucleation and growth, as compared with uncoated foams. Polyurethane foams with CNT coating have the potential to be used as bioactive scaffolds in bone tissue engineering due to their high interconnected porosity, bioactivity and nanostructured surface topography.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.