Abstract
AbstractPolythioureas having pendant hydroxyl groups were prepared by the polyaddition reaction of bisaminoalcohols and diisothiocyanates. The polythioureas had inherent viscosities in the range of 0.22–1.08 dl/g and gave transparent films by solution casting. These polythioureas were converted to polythiazolines by treatment with poly(phosphoric acid) or to poly(thiazoline–oxazolines) by treatment with a mixture of poly(phosphoric acid) and a polar solvent.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part A-1: Polymer Chemistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.