Abstract

AbstractEight biomedical glasses and three commercial glasses, as finely divided powders, were tested as initiators for the ring‐opening polymerization of ϵ‐caprolactone in bulk and in vacuo at 185°C. All the glass powders were able to initiate the polymerization, along with Pyrex, which was totally inert toward the monomer as the inner surface of a phial. The obtained polymers were examined with Fourier infrared transform spectroscopy and atomic force microscopy. The molecular weights were measured by viscometry in CHCl3. The presence of a fraction of the polymer firmly linked to the glass was quantitatively checked by the determination of the weight loss from the residues of the extraction with CHCl3 after calcination in a kiln at 945°C. The molecular weights and weight losses per unit surface were elaborated mathematically so that a possible correlation between these properties and the atomic compositions of the glasses could be better investigated. Two possible initiation mechanisms, induced by the hydroxyls present on the glass surface, were proposed: one for free poly(ϵ‐caprolactone) and one for poly(ϵ‐caprolactone) linked to the glass. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 87: 1579–1586, 2003

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call