Napier grass fibre was utilized for the development of biocomposite through nanocrystalline cellulose (NCC). NCC was generated by 64 wt% sulphuric acid in the hydrolysis cycle with 60 min time reaction. Biocomposite in film form has been prepared by mixing Poly (lactic acid) (PLA) and NCC using a method of solvent casting. In manufacturing of biocomposite films, NCC with different composition (0, 3, and 6 wt%) was used. The result of XRD analysis displayed an increase of crystallinity for PLA/NCC film compared to pure PLA film. However, PLA/NCC film with 6 wt% content of NCC (PLA/NCC-6) exhibited the highest percentage of crystallinity (69%). The chemical interaction of the structure between the NCC filler and the polymer matrix was studied using FTIR which confirmed by the presence of hydrogen bonding and the same trend of spectra was observed due to existence of PLA. PLA/NCC-3 demonstrated the lowest water absorption (0.37%) compared to pure PLA and PLA/NCC-6 film.KeywordsNanocrystalline celluloseBiocomposite filmNapier grass

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call