Abstract

ABSTRACTBiorenewable polyisoprene latex obtained from natural rubber, Hevea brasiliensis, was used to prepare the reusable polyisoprene–poly(alkyl acrylate) foam for petroleum‐based liquid absorption. The foam was produced via latex vulcanization and cured by steaming. The effect of various types of poly(alkyl acrylate) such as poly(methyl methacrylate) (PMMA), poly(butyl methacrylate) (PBMA), and poly(butyl acrylate) (PBA) on oil sorption capacity of the foam were studied. Scanning electron microscope (SEM) images showed interconnected open‐cell macrostructure with the foam porosity greater than 75% and good compression set. The oil sorption capacity of the foam was in the range of 2.0–16.6 g g−1. The addition of poly(alkyl acrylate) enhanced hydrophobicity and oil sorption capacity of the foam. The absorbed oil was easily recovered by squeezing and the foam can be reused up to 30 sorption–desorption cycles and still preserve high quality sorption. © 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 42688.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.