Abstract
Aim: This study evaluates the effect of electrospun dressings in critical sized full-thickness skin defects in rabbits. Materials & methods: Electrospun poly-ε-caprolactone (PCL) and polyvinyl alcohol (PVA) nanofibers were tested in vitro and in vivo. Results: The PCL scaffold supported the proliferation of mesenchymal stem cells, fibroblasts and keratinocytes. The PVA scaffold showed significant swelling, high elongation capacity, limited protein adsorption and stimulation of cells. Nanofibrous dressings improved wound healing compared with the control group in vivo. A change of the PCL dressing every 7days resulted in a decreased epithelial thickness and type I collagen level in the adhesive group, indicating peeling off of the newly formed tissue. In the PVA dressings, the exchange did not affect healing. Conclusion: The results demonstrate the importance of proper dressing exchange.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.