Abstract
Polymerization of coffee grounds oil with Diphenyl Methane 4,4 Diisocyanate (MDI), epoxidation with performic acid and H2SO4(p) catalyst at 40-45°C, followed by hydrolysis to obtain polyols. The synthesis was carried out by reacting the polyol with Diphenyl Methane 4,4 Diisocyanate (MDI) with a ratio (polyol: MDI) 9:1; 8:2 ; 7:3 ; 6:4 ; 5:5 (v/v) in dichloromethane solvent. Each was characterized and the density values were 0.9086 gr/cm to 0.4979 gr/cm-1, the tensile strength and elongation values were 0.113 Mpa to 0.299 Mpa and 3.23% to 6.85%, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.