Abstract
Corrosion properties of Sn-0.7Cu solder were investigated in 1 M HCl. The scanning rates used were 0.5, 1.0, 1.5 and 2.0 mVs-1 to study the aggressiveness level of HCl electrolyte in various environment. The morphological, elemental and structural of the samples were compared before and after the corrosion. Scan rate 1.0 mVs-1 was chosen as the most optimum scan rate during corrosion analysis. The morphological analysis observed two types of corrosion product which is compacted and loosely-compacted corrosion product after the samples was polarized in 1 M HCl.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.