Pb((Mg1/3Nb2/3)0.6(Fe1/2Nb1/2)0.4)O3 (PMFN) perovskite relaxor ferroelectric ceramics produced by reaction-sintering process were investigated. Without any calcination, the mixture of PbO, Mg(NO3)2, Fe(NO3)3 and Nb2O5 was pressed into pellets and sintered directly. PMFN ceramics of 100% perovskite phase were obtained. Density of 7.84 g/cm3 (95% of theoretical value) was obtained after sintered at 1250°C for 2 h. Grain sizes of 3–6 μm were formed after 2 h sintering at 1150–1250°C. Dielectric constant at room temperature under 10 kHz reaches 22400 after sintered at 1250°C for 2 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.