Abstract

The room temperature phase diagram of PLZT, (Pb,La)(Zr,Ti)O3, orL/Z/TforL<12 andT<10 was constructed using X‐ray diffraction patterns of sintered and crushed PLZT material. The orthorhombic antiferroelectric phase, a tetragonal phase, the rhombohedral (hexagonal) ferroelectric phases, and the mixed La‐rich zone were identified. Increasing substitution of La for Pb in the structure of orthorhombic PLZT leads to a change toward the cubic structure with less anisotropy in a direction corresponding to the cubic 200 direction. At La above ∼8 to 11 mol%, La2Zr2O7appears in the mixed zone. With increasing substitution of Ti for Zr, there is no change toward a cubic structure as the anisotropy is nearly unchanged. However, at a Ti substitution above ∼6 mol%, a rhombohedral and a tetragonal structure appear.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.