Abstract

AbstractThe present article discloses the properties improvement in PP/PA 6 blends by new type experimental coupling additives. By the experimental agents especially the tensile properties could be improved. For example, the tensile strength and the elongation were 16.5 MPa and 4.4% without additive, which increased to 25.5, 20.1, 46.8 MPa and 8.1, 6.4, 8.6% in specimens containing polyalkenyl‐poly‐maleic‐anhydride‐amide, polyalkenyl‐poly‐maleic‐anhydride‐ester, and MA‐grafted‐low‐polymer additives, respectively. DSC curves shows that compatibilizers influenced thermal properties of the polymer blends and reveal affecting of crystalline phase formation process in the blends due to the compatibilization step. Additives A and B rather leads to influencing of PA crystallinities. According to the SEM and FTIR analysis well separated polypropylene and polyamide phases was observed in case of specimens absence of additives but only one well distributed phase by the applying of the synthetized coupling agents. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call