Abstract
An appropriate synthesis technique for growing high-quality indium-free ZnSnOx (ZTO) films should be developed to achieve high-performance thin-film transistors (TFTs) utilizing ZTO films. This study investigated the growth characteristics and electrical properties of ZTO thin films grown via plasma-enhanced atomic layer deposition (PEALD) using bis(1-dimethylamino-2-methyl-2-propoxide)Sn, diethylzinc, and O2 plasma to optimize the composition and enhance the device performance. Deviations were observed in the growth per cycle when using PEALD for ZTO, compared with binary oxides. In the PEALD of the ZTO films, the introduction of the SnO2 sub-cycle enhanced the mass gain in the ZnO sub-cycle, whereas the mass gain in the SnO2 sub-cycle decreased with the addition of the ZnO sub-cycle. This was attributed to changes in the density of the functional groups on the reaction surface. Precise control over the composition was achieved, enabling the identification of the optimal Zn58Sn42Ox composition. Post-deposition annealing significantly improved the TFT performance, with devices showing enhanced mobility, positive shifts in the threshold voltage, and reduced subthreshold swing values. These improvements stemmed from reductions in oxygen vacancies and sub-gap defect states. These findings highlight the potential of PEALD-grown ZTO films for use in high-performance, cost-effective TFTs, facilitating their integration into modern semiconductor electronics.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Applied Surface Science
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.