Abstract

Sintered samples containing Mo, Ni and Mn, were plasma nitrided or nitrocarburized or sulphonitrocarburized with seven different cycles. After characterization the dry wear resistance of the treated samples was evaluated by an Amsler tribometer. The samples with the best wear resistance have a surface layer formed by martensite and retained austenite. A good wear resistance is also observed for the samples with a surface layer formed by a high amount of e solid solution, or e solid solution with a great carbon content. The samples with the worst wear resistance have the thinnest surface layers or with the lowest amount of e solid solution.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.