The article presents test results concerning the effect of a cladding method and technological process parameters on geometrical properties and dilution of overlay welds. Test overlay welds were deposited on tubes made of steel 13CrMo4-5. The chemical composition of the filler material used in the deposition process corresponded to that of alloy Inconel 625. The study involved the performance of macro and microscopic metallographic tests of the overlay welds as well as the identification of related dilution. The study also included hardness measurements involving the cross-section of the overlay welds as well as tests of the chemical composition of the overlay weld surface (paying attention to the maximum content of iron in the overlay weld, which should not exceed 5%). Adopted PTA and TOPTIG cladding parameters enabled the satisfaction of the maximum criterion related to the acceptable content of iron in the overlay weld, ensuring the stability of the cladding process and the invariable geometry of the overlay welds around the entire tube circumference.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.