Abstract

Silicon oxynitride films with varying oxygen/nitrogen ratio were grown from SiH4, N2O, and NH3 by means of a plasma-enchanced chemical vapor deposition process. The elemental composition of the deposited films was measured by a variety of high-energy ion beam techniques. To determine the chemical structure we used Fourier transform infrared absorption spectroscopy and electron-spin resonance. Ellipsometric data and values for mechanical stress are also reported. We show that the entire range of compositions from silicon oxide to silicon nitride can be covered by applying two different processes and by adjusting the N2O/NH3 gas flow ratio of the respective processes. It is suggested that the N2O/SiH4 gas flow ratio is the major deposition characterization parameter, which also controls the chemical structure as far as the hydrogen bonding configuration is concerned. We found that the films contain significant amounts of excess silicon and that the mechanical stress in the oxynitrides is lower than in plasma nitride. The electron-spin density is low (∼1017/cm3) in all samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.