Abstract
Abstract Single crystals of a copper-beryllium alloy of two axial orientations ([111] and [110]) strained in tension showed slip on (111/ planes. The same crystals, stressed in tension and exposed to an ammonia atmosphere, failed in a transcrystalline mode. In crystals of [111] orientation cracks propagated on (123) planes. Calculations show that in these crystals, the maximum resolved shear stress on the (111) slip planes is produced when the crack propagates on the (123) plane. In crystals of the [110] axial orientation, the cracks propagated on (110) planes. Again calculations show that the maximum resolved shear stress on the (111) slip planes is produced when the crack propagates on the (110) plane. These results indicate that crack propagation occurred on planes which would result in the maximum plastic deformation on the available slip system.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.