Two types of inclusions in the stainless steels are detected: MnO·Cr2O3–MnS dual‐phase ones and pure MnS ones. The increase of sulfur content can inhibit the formation of MnO–Cr2O3–MnS inclusions and reduce the harm of MnO·Cr2O3–MnS inclusions on the pitting corrosion of stainless steels. When the sulfur content increases from 26 to 70 ppm, the average pitting potential increases from 0.34 to 0.4 VSCE due to the decrease in the number density of MnO–Cr2O3–MnS inclusions. A Cr‐depletion zone exists in the steel matrix around MnO–Cr2O3–MnS inclusions. The size of pits induced by MnO·Cr2O3–MnS inclusions is larger, which poses a more serious threat to the pitting resistance of stainless steels.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.