Abstract
The corrosion behavior of surgical implant CoCr alloy and REX 734 steel has been investigated. The pitting or crevice corrosion potentials have been determined to reach values as high as 500mV vs. SCE for CoCr and 450mV vs. SCE for REX 734. The galvanic corrosion behavior of CoCr/REX 734 couples has been evaluated with various electrochemical techniques. The measurement of the corrosion current of the galvanic couple as well as its prediction by applying mixed potential theories on measured potentiodynamic polarization curves revealed low galvanic currents in the range of nanoamperes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.