Abstract

Conducting polymers of polyaniline (PANi) and poly(o-phenylenediamine) (PoPD) were electropolymerized by cyclic voltammetric technique on low nickel stainless steel (LN SS) in H2SO4solution containing aniline and o-phenylenediamine monomers. The coatings were characterized by Fourier transform infrared spectroscopy, UV-visible and scanning electron microscopic techniques and the results are discussed. The corrosion protective properties of PANi and PoPD coatings on LN SS in 0·5 M NaCl were evaluated using potentiodynamic polarization and electrochemical impedance spectroscopic (EIS) techniques. The potentiodynamic polarization and electrochemical impedance spectroscopic results indicate that the PoPD coating inhibits the corrosion of LN SS in 0·5 M NaCl solution more effectively than PANi.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.