The pitting corrosion behavior of the melt-spun amorphous Ni-Zr alloys with 30-75 at% zirconium, the crystalline arc-melted counterparts and the sputter-deposited Ni-Zr alloys with 20-84 at% zirconium was examined by electrochemical measurements in deaerated 0.5 kmol/ m 3 H 2 SO 4 with and without 0.1 kmol/m 3 NaCl at 303 K. In the sulfuric acid solution without Cl - , these alloys were spontaneously passive and their potentiodynamic behavior was similar to each other. In the Cl - -containing solution, all the melt-spun amorphous alloys suffered pitting during anodic polarization and the pitting potential decreased with an increase in zirconium content. On the other hand, the crystalline arc-melted low zirconium alloys suffered pitting but no pitting observed for the crystalline alloys containing 70 at% zirconium or more. In addition, the pitting potential increased with the zirconium content of crystalline alloys. All the sputter-deposited alloys did not suffer pitting regardless of the amorphous and crystalline structures. Therefore, the melt-spun amorphous alloys were the most susceptible to pitting corrosion. A marked difference was observed in the pitting behavior between the shiny side (top side) and the dull side (wheel side) surfaces of the melt-spun ribbon. The pits initiated from the dull side surface. Thus, the dull side surface could be responsible for such an unusual pitting behavior of the melt spun ribbon.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call