Abstract

This review describes the experiments performed during the last few decades which enhance knowledge of the pitting of aluminum. Specifically, metastable and stable pits, pit chemistry and the effect of intermetallics on pitting are discussed. The properties of metastable alloys and inhibition of Al are also discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.