Abstract
Abstract This paper presents a research on the corrosion behavior of Ti-15-3 alloy overlapped with aluminized PVC film in salt spray. It was found that severe corrosion occurred on aluminized PVC film in the coupled regions because of crevice corrosion and/or galvanic corrosion whereas Ti-15-3 alloy in the coupled regions experienced minor corrosion. Scanning electron microscope and Energy-dispersive X-ray spectroscopy analyses demonstrated the corrosion products adhered to the surface of Ti-15-3 alloy within the crevice. To evaluate the effect of aluminized PVC film on the crevice corrosion of Ti-15-3 alloy in salt spray condition, it is necessary to compare with the corrosion resistance of Ti-15-3 overlapped with polytetrafluoroethylene (PTFE) in different neutral salt spray. Further, the tests were performed by electrochemical impedance spectroscopy and potentiodynamic polarization. Combining the graphical model, an in-depth understanding of the crevice and galvanic corrosion mechanism of Ti-15-3 alloy overlapped with aluminized PVC film has been revealed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.