Micropits surrounded by coloured halos were observed under incident-light microscope on 1Cr18Ni9Ti stainless steel surface after “ennoblemen t” in seawater. Ennoblement has been attributed to biofilm formation on stainless steel surface in seawater. In this study, the environment in biofilm for ennoblement was simulated by adding H 2O 2 into seawater at concentrations that were reported to detect in marine biofilm [N. Washizu, Y. Katada, T. Kodama, Corros. Sci .46 (2004)1291.]. H 2O 2 increased the passivity of stainless steel in seawater, but this passivation was not uniform. The probability of pitting corrosion was increased after ennoblement. Equal thickness interference on the deposition film around the pits was believed to be the reason for the coloured fringes. It is conceivable that haloed pits on the stainless steel surface are the characteristic morphological indications for pitting corrosion formed under ennoblement condition in seawater. Examinations on the microbial and structural effects of the biofilm were not included in this study.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.