Abstract

Zinc oxide (ZnO) thin films are deposited by plasma‐enhanced atomic layer deposition (PE‐ALD). This deposition method allows depositing stoichiometric and highly resistive ZnO films at room temperature. Despite such important requirements for piezoelectricity being met, not much is known in literature about the piezoelectric properties of ZnO thin films (<70 nm) deposited by PE‐ALD. The films are grown at different substrate temperatures to investigate the effect on crystalline and piezoelectric properties. Films deposited on flexible poly(ethylene terephthalate) (PET) generated a higher piezoelectric current (>1.8 nA) and charge (>80 pC) compared with films deposited on glass (>0.3 nA and >30 pC) due to bending effects of the substrate when mechanically excited. Furthermore, increasing the substrate temperature, during deposition, enhances the growth along the (002) crystallographic orientation, which further strengthens the generated piezoelectric current signal for mechanical excitations along the ZnO film's c‐axis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.