Abstract

The ternary piezoelectric material Pb0.97Sr0.03[Zr0.458Ti0.452(Mn1/3Nb2/3)0.09]O3 in the tetragonal phase near the morphotropic phase boundary (MPB) was prepared in this study. By properly varying the sintering and poling conditions, the zero temperature coefficient of the resonant frequency of the thickness vibration mode can be reached due to the slight shift of the MPB region. The computed Bechmann number based on the principle of trapped energy revealed that the high-frequency resonators with electrode width of at least less than 1 mm are suggested corresponding to the plate thickness of 0.205 mm to exhibit better resonance performance due to the suppression of unwanted mode coupling.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.