Abstract

The physico-mechanical properties of degradable polymers used for medical applications have been characterized. The following polymers were included in this study: three samples of poly(ortho esters) derived from 3,9-bis(ethylidene 2,4,8,10-tetraoxaspiro[5,5]undecane) and various ratios of 1,6-hexanediol and trans-cyclohexane dimethanol, poly(glycolic acid), six samples of poly( l-lactic acid) and poly( d,l-lactic acid) with mol wt from 21 000 to 550 000, poly(ε-caprolactone), poly(β-hydroxybutyrate) and three copolymers of β-hydroxybutyric acid and various amounts of hydroxyvaleric acid, one sample each of two different types of poly(anhydrides), poly(trimethylene carbonate) and two different poly(iminocarbonates). For each polymer, the thermal properties (glass transition temperature, crystallization, melting and decomposition points) were determined by differential scanning calorimetry and by thermogravimetric analysis. The tensile properties (Young's modulus, tensile strength and elongation at yield and break) were determined by tensile testing on an Instron stress-strain tester. The flexural storage modulus as a function of temperature was determined by dynamic mechanical analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.