Abstract

Due to limitations of bone autografts and allografts, synthetic bone grafts using osteoconductive biomaterials have been designed. In this study, collagen-chitosan-calcium phosphate microparticle-based scaffolds fused with glycolic acid were compared to their counterparts without collagen in terms of degradation, cytocompatibility, porosity, and Young's modulus. It was found that 26-30% collagen was incorporated and that hydroxyapatite was present. Moreover, there were no differences between control and collagen scaffolds in degradation, cytocompatibility, porosity, and Young's modulus. In general, scaffolds exhibited 23% porosity, 0.6-1.2 MPa Young's modulus, 23% degradation over 4 weeks, and supported a four to seven fold increase in osteoblast cell number over 7 days in culture. Collagen can be incorporated into these bone graft substitute scaffolds, which show an improved degradation profile.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.