Abstract

The current work reports on the fabrication of composite matrix from saw dust (SD) and recycled polyethylene terephthalate (PET) at different weight ratio by flat-pressed method. Wood plastic composites (WPCs) were made with a thickness of 15 mm after mixing the saw dust and PET followed by a three phase press cycle. Physical properties (Density, Water Absorption (WA) and Thickness Swelling (TS)) and Mechanical properties (Modulus of Elasticity (MOE) and Modulus of Rupture (MOR)) were determined base on the mixing ratios according to the standard. WA and TS were measured after 2 h and 24 h of immersion in water. The results showed that as the density increased, the SD content decreased from 90 % to 50 % into the matrix. However, WA and TS decreases when the PET content increased in the matrix. Remarkably, the MOE and MOR attained a maximum point at 964.199 N/mm2and 9.03 N/mm2respectively in 50 % SD content. In comparism with standard, boards D and E can be classified as medium density boards while A, B and C are low density boards. The results indicated that the fabrication of WPCs from sawdust and PET would technically be feasible for indoor uses in building due to favorable physical properties exhibited. The mechanical properties response showed that it cannot be used for structural or load bearing application.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.