Abstract

We have grown epitaxial anatase-TiO2 (001) films on La0.5Sr0.5CoO3 (001) bottom electrodes using pulsed-laser deposition. The small lattice mismatch (0.5%) between the anatase-TiO2 and the La0.5Sr0.5CoO3 makes it possible to grow anatase-TiO2 films with excellent crystallinity on conductive metal oxides. The photovoltaic properties of the epitaxial anatase-TiO2 on the La0.5Sr0.5CoO3 were characterized using a Kelvin probe. The optical band-gap energy was found to be 3.05 eV. The dielectric properties of the epitaxial anatase-TiO2 films were characterized using a capacitor structure of Au/anatase-TiO2/La0.5Sr0.5CoO3 on a LaAlO3 substrate. The dielectric dispersion exhibited a power-law dependence, and the dielectric constant measured at room temperature and 1 MHz was 38.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.