Abstract

We demonstrate phototriggered depolymerization of a low ceiling temperature ( Tc) polymer, poly(phthalaldehyde) (PPHA), via internal light emission from integrated organic light-emitting diodes (OLEDs) fabricated directly on flexible PPHA substrates with silver nanowire electrodes. The depolymerization of the PPHA substrates is triggered by absorption of the OLED emission by a sensitizer that activates a photoacid generator via energetically favorable electron transfer. We confirm with Fourier-transform infrared spectroscopy that the photon doses delivered by the integrated OLED are sufficient to depolymerize the PPHA substrates. We determine this critical dosage by measuring the operating lifetimes of the OLEDs whose failure is believed to be due to significant mechanical softening during the liquefaction of decomposed phthalaldehyde monomers.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.