The materials ratio is compounded followed by the molecular formula Ba 0.5 Sr 1.5 K 0.5 Na 0.5 Nb 5 O 15 . Doping 0.05 wt% CeO 2 and 0.03 wt% Co 2 O 3 in KNSBN, Ce:Co:KNSBN crystal was grown by Czochralski technique adopting SiMo heater furnace. The exponential gain coefficient, diffraction efficiency and response time of Ce:Co:KNSBN crystal were measured through two-beam couple light path. The phase conjugation reflect efficiency and response time of Ce:Co:KNSBN and Cu:SBN crystals were measured by four-wave mixing light path. The holographic associative storage were established by using Ce:Co:KNSBN crystal as recording apparatus and Cu:SBN crystal as phase conjugation lens. Addressing was operated by 75% and 50% images and the associative storage reappearing images are clear, complete and noise was small. The photo-refractive effects of Ce:Co:KNSBN crystal are more excellent than KNSBN crystal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call