Abstract Pure and peroxided PVC films were irradiated under monochromatic ultraviolet light between 300 and 400 nm. The degradation state of PVC is measured by means of carbonyl absorption in the infrared spectra and polyene content by UV spectroscopy. The initial rate of carbonyl formation depends on the wavelengths and oxidized impurities content. Peroxided PVC is oxidized faster than pure PVC with wavelengths above 320 nm. Two hazardous ranges of wavelengths have been detected: 300–320 and 350–370 nm. Good protection of PVC against UV radiation can be assured by the exclusion of wavelengths under 380 nm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Macromolecular Science: Part A - Chemistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.