Abstract

While the industry is making progress to offer EUV lithography schemes to attain ultimate critical dimensions down to 20 nm half pitch, an interim optical lithography solution to address an immediate need for resolution is offered by various integration schemes using advanced PSM (Phase Shift Mask) materials including thin e-beam resist and hard mask. Using the 193nm wavelength to produce 10nm or 7nm patterns requires a range of optimization techniques, including immersion and multiple patterning, which place a heavy demand on photomask technologies. Mask schemes with hard mask certainly help attain better selectivity and hence better resolution but pose integration challenges and defectivity issues. This paper presents a new photomask etch solution for attenuated phase shift masks that offers high selectivity (Cr:Resist > 1.5:1), tighter control on the CD uniformity with a 3sigma value approaching 1 nm and controllable CD bias (5-20 nm) with excellent CD linearity performance (<5 nm) down to the finer resolution. The new system has successfully demonstrated capability to meet the 10 nm node photomask CD requirements without the use of more complicated hard mask phase shift blanks. Significant improvement in post wet clean recovery performance was demonstrated by the use of advanced chamber materials. Examples of CD uniformity, linearity, and minimum feature size, and etch bias performance on 10 nm test site and production mask designs will be shown.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.