Abstract

In this study, Sm 3+ - and Dy 3 -doped SrAl4O7 phosphors were synthesized by combustion method. X-ray diffraction (XRD) measurement confirmed the monoclinic crystal structure of SrAl4O7. Sr-O and Al-O bonds were identified by Fourier transform infrared (FTIR) spectroscopy. Under 352 nm excitation, the SrAl4O7: Dy 3+ phosphor shown emission bands at 475 nm (blue) and 574 nm (yellow) that are due to 4 F9/2→ 6 H15/2, 6 H13/2 transitions, respectively. Photoluminescence spectra (PL) of SrAl4O7: Sm 3+ phosphor has shown bright orange red emission at 598 nm with an excitation wavelength of 405 nm. The decay curve of Sm 3+ and Dy 3+ single doped SrAl4O7 phosphors were well fitted to a bi-exponential function. The obtained results show that the prepared phosphors may be applicable in the field of eco-friendly solid state lighting technology. Copyright © 2015 VBRI Press.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.