Two kinds of porous ceramic disks, having through-holes with diameters of 0.1 and 0.05 mm, were coated with TiO2 using two different starting solutions: titanyl(IV)acetylacetonate and a commercial titania sol (STS-01). The morphology of these porous ceramics before and after TiO2 coating was observed by SEM. The TiO2-coated porous ceramics were examined as honeycomb photocatalytic microreactors. The photocatalytic activity was evaluated using the decomposition of methylene blue solution for radiation angles of 0° and 10° with respect to the pore axis. The highest photocatalytic activity was obtained for the porous ceramic having the pore diameter of 0.1 mm, coated with titanyl(IV)acetylacetonate and irradiated with a light angle of 0° with respect to the pore axis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.