Abstract

ZnO–bentonite nanocomposite was obtained by incorporation of bentonite clay with ZnO. The effects of pH, contact time, initial dye concentration and photocatalyst dose on the rate of degradation of dye solution were studied. It was observed that working conditions strongly influence the dye removal process. Contact time 70 min and pH 4 was optimized for photocatalytic degradation of Safranine. Adsorption kinetics for 20–80 mg/l dye concentration was found to follow pseudo-second-order kinetics. Adsorption of dye was described by Langmuir and Freundlich isotherm. In adsorption isotherm, Langmuir isotherm was found to fit well with experimental data than Freundlich isotherm. The monolayer adsorption capacity was found to be 50 mg/g. The amount of dye adsorbed (q t ) increases from 17.31 to 159.62 mg/g as dye concentration increases from 20 to 80 mg/l for 0.4 g/l photocatalyst dose. The photocatalytic degradation of Safranine by ZnO–bentonite takes place by advanced oxidation process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.