Abstract

The photocatalytic performance of mechano-thermally synthesized Fe/FeS nanostructures formed from micron-sized starting materials was compared with that of a thermally synthesized nanostructure with nano-sized precursors in this paper. The properties of as-synthesized materials were studied by X-ray diffraction (XRD), transmission electron microscopy (TEM), vibrating sample magnetometry (VSM), diffuse reflectance spectroscopy (DRS), and ultraviolet-visible (UV-Vis) spectroscopy. The effects of irradiation time, methylene blue (MB) concentration, catalyst dosage, and pH value upon the degradation of MB were studied. Magnetic properties of the samples showed that both as-synthesized Fe/FeS photocatalysts are magnetically recoverable, eliminating the need for conventional filtration steps. Degradation of 5 ppm of the MB solution by mechano-thermally synthesized Fe/FeS with a photocatalyst dosage of 1 kg/m3 at pH 11 can reach 96% after 12 ks irradiation under visible light. The photocatalytic efficiency is higher in alkaline solution. The kinetics of photocatalytic degradation in both samples is controlled by a first-order reaction. However, the rate-constant value in the thermally synthesized Fe/FeS photocatalyst sample is only 1.5 times greater than that of the mechano-thermally synthesized one.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.