Abstract

We have experimentally determined loss coefficients of OH as 8.1 × 10−7 cm−1 / ppm and of ionic platinum as 8.6 × 10−7-7cm−1/ppm for LHG-5 type phosphate laser glass without Nd2O3 doping. Glass has been produced with absorption loss of about 1 ×c 10−4cm−1 which is one order of magnitude lower than is presently commercially available.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.