Fine-grained tungsten (W) heavy alloy containing molybdenum (Mo) with W particle sizes of less than 5μm were fabricated by spark plasma sintering (SPS) pre-milling W–2Mo–7Ni–3Fe powder at a lower temperature of 1000–1250°C. Phase, microstructure and mechanical properties evolution of W–Mo–Ni–Fe alloy during spark plasma sintering were studied in detail. As increasing sintering temperature, the hardness of the alloy decreased rapidly. However, bending strength of the alloy demonstrated a fall–rise–fall trend, and the maximum strength was obtained at 1150°C. The W–2Mo–7Ni–3Fe alloy microstructure was composed of white W-grain, gray W-rich structure, black γ-(Ni, Fe, W, Mo) binding phase, and deep-gray W-rich structure. The intergranular fracture along the W/W grain boundary is the main fracture modes of W–2Mo–7Ni–3Fe alloy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.