We successfully synthesized bulk Ba0.6Na0.4Fe2As2 and Sr0.5Na0.5Fe2As2 compounds by high-energy mechanical alloying (MA) technique. The MA process results in homogeneous amorphous phases of BaFe2As2 and SrFe2As2. It was found that the optimum time for high-energy milling in all cases is about 1.5-2 h, and the maximum amount of amorphous phase could be obtained when energy of 50-100 MJ/kg was absorbed by the powder. After a short-term heat treatment, we obtained nearly optimum sodium-doped Ba1-xNaxFe2As2 and Sr1-xNaxFe2As2 superconducting bulk samples. Therefore, MA is a potential scalable method to produce bulk superconducting material for industrial needs.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.